N2 - This paper reports the elastic constants of the Ni-base single crystal superalloy (TMS-26) with a rafted (lamellar) structure having tetragonal symmetry. The elastic constants have been measured at room temperature with the resonance ultrasound spectroscopy method and the mode-selective electromagnetic acoustic resonance method. The value of the elastic constant c33 (250.4 GPa) is almost equal to that of c11 (252.5 GPa), which indicates that the rafted structure virtually has the elastic anisotropy of cubic system.
AB - This paper reports the elastic constants of the Ni-base single crystal superalloy (TMS-26) with a rafted (lamellar) structure having tetragonal symmetry. The elastic constants have been measured at room temperature with the resonance ultrasound spectroscopy method and the mode-selective electromagnetic acoustic resonance method. The value of the elastic constant c33 (250.4 GPa) is almost equal to that of c11 (252.5 GPa), which indicates that the rafted structure virtually has the elastic anisotropy of cubic system.
KW - Electromagnetic acoustic resonance
KW - Ni-base single crystal superalloy
KW - Rafted structure
KW - Resonant ultrasonic spectroscopy
KW - Vibration mode
UR - http://www.scopus.com/inward/record.url?scp=0036566283&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=0036566283&partnerID=8YFLogxK
U2 - 10.1016/S0041-624X(02)00139-7
DO - 10.1016/S0041-624X(02)00139-7
M3 - Article
AN - SCOPUS:0036566283
SN - 0041-624X
VL - 40
SP - 211
EP - 215
JO - Ultrasonics
JF - Ultrasonics
IS - 1-8
ER -