Highly transparent lutetium titanium oxide produced by spark plasma sintering

Liqiong An, Akihiko Ito, Takashi Goto

Research output: Contribution to journalArticlepeer-review

42 Citations (Scopus)

Abstract

Transparent Lu2Ti2O7 pyrochlore was fabricated by reactive sintering using spark plasma sintering at 1723K for 45min. The sintered body exhibited 72% transmittance at a wavelength of 2000nm and 40% transmittance at 550nm. The average grain size was 14.5μm with uniform microstructure.

Original languageEnglish
Pages (from-to)237-240
Number of pages4
JournalJournal of the European Ceramic Society
Volume31
Issue number1-2
DOIs
Publication statusPublished - 2011 Jan 1

Keywords

  • LuTiO
  • Pyrochlore
  • Spark plasma sintering
  • Transparent ceramic