N2 - We describe low-loss silica photonic crystal fiber fabricated by a slurry casting method with an OH reduction process that provides a highly flexible air-hole structure and a low fabrication cost. The loss was 1.1 dB/km at 1.55 mm.
AB - We describe low-loss silica photonic crystal fiber fabricated by a slurry casting method with an OH reduction process that provides a highly flexible air-hole structure and a low fabrication cost. The loss was 1.1 dB/km at 1.55 mm.
UR - http://www.scopus.com/inward/record.url?scp=84890689255&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=84890689255&partnerID=8YFLogxK
U2 - 10.1364/cleo_si.2012.cth3g.1
DO - 10.1364/cleo_si.2012.cth3g.1
M3 - Conference contribution
AN - SCOPUS:84890689255
SN - 9781557529435
T3 - CLEO: Science and Innovations, CLEO_SI 2012
SP - CTh3G.1
BT - CLEO
PB - Optical Society of America (OSA)
T2 - CLEO: Science and Innovations, CLEO_SI 2012
Y2 - 6 May 2012 through 11 May 2012
ER -