6.5% silicon steel sheets with almost (100) texture can be obtained by using two methods of Method's A and B. In Method A, 6.5% silicon sheets were annealed in the vacuum of 1.0 Pa after dipping the sheets in sulfur solution. In Method B, an annealing in the vacuum of 1.0×10-4 Pa was added before the process of Method A. In the samples fabricated by Method B, the average magnetic induction of 800 A/m, B8=1.39 T was larger than that of the conventional 6.5% silicon sheets (05EX2500 NKK corporation) by about 0.1 T.

Original languageEnglish
Pages (from-to)745-748
Number of pages4
JournalMaterials Science Forum
Volume373-376
DOIs
Publication statusPublished - 2001
Event8th European Magnetic Materials and Applications Conference (EMMA 2000) - Kyiv, Ukraine
Duration: 2000 Jun 72000 Jun 10

Keywords

  • (100) texture
  • 6.5% silicon steels
  • B
  • Sulfur solution

Fingerprint

Dive into the research topics of 'Preparation of 6.5% silicon steel sheets with (100) texture'. Together they form a unique fingerprint.

Cite this