TY - JOUR
T1 - Structural and electrical characterization of hydrothermally deposited piezoelectric (K,Na)(Nb,Ta)O3 thick films
AU - Shiraishi, Takahisa
AU - Muto, Yuta
AU - Ito, Yoshiharu
AU - Kiguchi, Takanori
AU - Sato, Kazuhisa
AU - Nishijima, Masahiko
AU - Yasuda, Hidehiro
AU - Funakubo, Hiroshi
AU - Konno, Toyohiko J.
N1 - Funding Information:
This research was partially supported by the Japan Science and Technology Agency (JST) via the Adaptable and Seamless Technology Transfer Program through Target driven R&D (A-STEP) Grant Number JPMJTS1616. In addition, this work was supported by Yashima Environment Technology Foundation. A part of this work was supported by “Advanced Characterization Nanotechnology Platform, Nanotechnology Platform Program of the Ministry of Education, Culture, Sports, Science and Technology (MEXT), Japan” at the Research Center for Ultra-High Voltage Electron Microscopy (Nanotechnology Open Facilities) in Osaka University (Project number: A-17-OS-0042).
Publisher Copyright:
© 2020, Springer Science+Business Media, LLC, part of Springer Nature.
PY - 2020/7/1
Y1 - 2020/7/1
N2 - (K0.89Na0.11)(Nb0.85Ta0.15)O3 thick films were epitaxially grown at 200 °C on (001)La:SrTiO3 and (001)cSrRuO3//(001)SrTiO3 substrates by hydrothermal method, and their crystal structures and electrical properties were investigated.Film thickness increased with deposition time and reached 6 µm in 10 h. High-temperature X-ray diffraction measurement showed that successive phase transitions from orthorhombic to tetragonal and from tetragonal to cubic phases take place at 120 and 400 °C, respectively. Microstructure analyses were performed by using electron microscopy, which revealed the existence of two types of stripe patterns with a width of 100 nm or less. In addition, scanning transmission electron microscopy–energy-dispersive X-ray spectroscopy elemental mapping showed that Nb/(Nb + Ta) ratio of the deposited films abruptly changed around 700 nm in thickness. Annealing at 500 °C led to the reduction in leakage current density from 102 to 10–5 A/cm2 at 30 kV/cm, showing that annealing is an effective way to improve insulation. Relative dielectric constant (εr) decreased linearly with increasing frequency, reaching 450 at 10 kHz. Polarization–electric field hysteresis loop and field-induced stain curve were measured by piezoelectric force microscopy, which showed remanent polarization (Pr) of 30 µC/cm2 and piezoelectric constant (d33,PFM) of 70 pm/V. These results demonstrate that (K,Na)(Nb,Ta)O3 thick films with superior electrical properties can be fabricated by the low-temperature deposition technique.
AB - (K0.89Na0.11)(Nb0.85Ta0.15)O3 thick films were epitaxially grown at 200 °C on (001)La:SrTiO3 and (001)cSrRuO3//(001)SrTiO3 substrates by hydrothermal method, and their crystal structures and electrical properties were investigated.Film thickness increased with deposition time and reached 6 µm in 10 h. High-temperature X-ray diffraction measurement showed that successive phase transitions from orthorhombic to tetragonal and from tetragonal to cubic phases take place at 120 and 400 °C, respectively. Microstructure analyses were performed by using electron microscopy, which revealed the existence of two types of stripe patterns with a width of 100 nm or less. In addition, scanning transmission electron microscopy–energy-dispersive X-ray spectroscopy elemental mapping showed that Nb/(Nb + Ta) ratio of the deposited films abruptly changed around 700 nm in thickness. Annealing at 500 °C led to the reduction in leakage current density from 102 to 10–5 A/cm2 at 30 kV/cm, showing that annealing is an effective way to improve insulation. Relative dielectric constant (εr) decreased linearly with increasing frequency, reaching 450 at 10 kHz. Polarization–electric field hysteresis loop and field-induced stain curve were measured by piezoelectric force microscopy, which showed remanent polarization (Pr) of 30 µC/cm2 and piezoelectric constant (d33,PFM) of 70 pm/V. These results demonstrate that (K,Na)(Nb,Ta)O3 thick films with superior electrical properties can be fabricated by the low-temperature deposition technique.
UR - http://www.scopus.com/inward/record.url?scp=85083794774&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=85083794774&partnerID=8YFLogxK
U2 - 10.1007/s10853-020-04663-x
DO - 10.1007/s10853-020-04663-x
M3 - Article
AN - SCOPUS:85083794774
SN - 0022-2461
VL - 55
SP - 8829
EP - 8842
JO - Journal of Materials Science
JF - Journal of Materials Science
IS - 21
ER -