Abstract
The recovery of SiO2 and Al2O3 from the alkali waste solution of the glass polishing powder-recycling process was investigated. The effects of seed crystal, stirring speed, and temperature were also studied. Hydroxysodalite was obtained from the waste solution by heating to 80-100 °C. Addition of seed crystal shortened the reaction time and made easy the recovery of hydroxysodalite. The hydroxysodalite deposition process was rate-determined by the chemical reaction step, and increased temperature was also effective in shortening a reaction time.
Original language | English |
---|---|
Pages (from-to) | 4148-4151 |
Number of pages | 4 |
Journal | Industrial and Engineering Chemistry Research |
Volume | 39 |
Issue number | 11 |
DOIs | |
Publication status | Published - 2000 |