TY - JOUR
T1 - Synthesis and properties of ferromagnetic Fe-based (Fe, Ni, Co)-Mo-P-C-B bulk metallic glasses with large supercooled liquid region
AU - Jia, Xingjie
AU - Li, Yanhui
AU - Wang, Hao
AU - Xie, Guoqiang
AU - Yamaura, Shinichi
AU - Zhang, Wei
N1 - Funding Information:
This research was supported by the National Natural Science Foundation of China (Grant nos. 51271043 , 51171034 , and 51201024 ), and the Research Fund for the Doctoral Program of Higher Education (Grant no. 20130041110006 ).
Publisher Copyright:
© 2015 Elsevier B.V.Allrights reserved.
PY - 2015/5/26
Y1 - 2015/5/26
N2 - New ferromagnetic Fe-based (Fe, Co, Ni)67.5Mo7.5P10C10B5 bulk metallic glasses have been developed based on an Fe75P10C10B5 alloy. These alloys exhibit large supercooled liquid region of 97-102 K, low glass transition temperature of 727-738 K, high glass-forming ability (GFA) with critical sample diameters of 3-4 mm, and low viscosity values on the order of 107 Pa s in the supercooled liquid state. The magnetic and mechanical measurements reveal that the alloys also possess good soft magnetic and mechanical properties, i.e., low coercive force of 3.04-4.37 A/m, rather high saturation magnetization of 0.77-0.83 T, high yield strength of 3344-3463 MPa, and large plastic strain of 0.6-1.1%. In addition, the effects of Mo, Co and Ni addition on the stabilization of supercooled liquid and GFA in the Fe-P-C-B alloy system have been discussed.
AB - New ferromagnetic Fe-based (Fe, Co, Ni)67.5Mo7.5P10C10B5 bulk metallic glasses have been developed based on an Fe75P10C10B5 alloy. These alloys exhibit large supercooled liquid region of 97-102 K, low glass transition temperature of 727-738 K, high glass-forming ability (GFA) with critical sample diameters of 3-4 mm, and low viscosity values on the order of 107 Pa s in the supercooled liquid state. The magnetic and mechanical measurements reveal that the alloys also possess good soft magnetic and mechanical properties, i.e., low coercive force of 3.04-4.37 A/m, rather high saturation magnetization of 0.77-0.83 T, high yield strength of 3344-3463 MPa, and large plastic strain of 0.6-1.1%. In addition, the effects of Mo, Co and Ni addition on the stabilization of supercooled liquid and GFA in the Fe-P-C-B alloy system have been discussed.
KW - Iron-based alloys
KW - Mechanical properties
KW - Metallic glasses
KW - Soft magnetic properties
KW - Viscosity
UR - http://www.scopus.com/inward/record.url?scp=84929710369&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=84929710369&partnerID=8YFLogxK
U2 - 10.1016/j.physb.2015.05.004
DO - 10.1016/j.physb.2015.05.004
M3 - Article
AN - SCOPUS:84929710369
SN - 0921-4526
VL - 470-471
SP - 107
EP - 112
JO - Physica B: Condensed Matter
JF - Physica B: Condensed Matter
ER -