N2 - Magnetization was measured in plastically deformed 37.0 at.% Al-Fe compounds in the temperature range from 4.5 to 61 K. Plastic deformation makes the spin-glass state increase; the frozen temperature changes from 32 to 37.5 K with 10% strain. The APB between superpartial dislocations plays an important role in this enhancement.
AB - Magnetization was measured in plastically deformed 37.0 at.% Al-Fe compounds in the temperature range from 4.5 to 61 K. Plastic deformation makes the spin-glass state increase; the frozen temperature changes from 32 to 37.5 K with 10% strain. The APB between superpartial dislocations plays an important role in this enhancement.
UR - http://www.scopus.com/inward/record.url?scp=0001215859&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=0001215859&partnerID=8YFLogxK
U2 - 10.1016/S0375-9601(05)80016-7
DO - 10.1016/S0375-9601(05)80016-7
M3 - Article
AN - SCOPUS:0001215859
SN - 0375-9601
VL - 197
SP - 350
EP - 352
JO - Physics Letters, Section A: General, Atomic and Solid State Physics
JF - Physics Letters, Section A: General, Atomic and Solid State Physics
IS - 4
ER -