Wettability of Ni-V, Co-V, and Ni-Cr-V system brazing alloys on Si3N4 ceramic and interfacial reactions

Hua Ping Xiong, Wei Dong, Bo Chen, Yan Sheng Kang, Akira Kawasaki, Hiroshi Okamura, Ryuzo Watanabe

Research output: Contribution to journalArticlepeer-review

25 Citations (Scopus)

Abstract

In the present paper, six V-active brazes were designed. The wetting behavior of Ni-V, Co-V and Ni-Cr-V alloys on Si3N4 was studied by the sessile drop method. The results show that, under the heating condition of 1553 K/120 min, the Ni-V alloys with the V content of no higher than 25 wt.% did not wet Si3N4, whereas, the Ni-V alloys with the V content of no lower than 34.5 wt.% exhibit good wettability. Though the spreading of the Ni-V, Co-V and Ni-Cr-V brazing alloys on the Si3N4 was slow, intensive interfacial reactions occurred, and according to the results of XRD analysis, compounds of V3Ni2Si, V6Si5 and VN were formed at the interface of Si3N4/Ni-V alloy. The corresponding interfacial reactions were also discussed.

Original languageEnglish
Pages (from-to)376-381
Number of pages6
JournalMaterials Science and Engineering A
Volume474
Issue number1-2
DOIs
Publication statusPublished - 2008 Feb 15
Externally publishedYes

Keywords

  • Brazing alloy
  • Interfacial reaction
  • SiN
  • Wettability

ASJC Scopus subject areas

  • Materials Science(all)
  • Condensed Matter Physics
  • Mechanics of Materials
  • Mechanical Engineering

Fingerprint

Dive into the research topics of 'Wettability of Ni-V, Co-V, and Ni-Cr-V system brazing alloys on Si3N4 ceramic and interfacial reactions'. Together they form a unique fingerprint.

Cite this