Characteristic energy band values and electron attenuation length of a chemical-vapor-deposition diamond (0 0 1)2 × 1 surface

S. Kono, T. Saitou, H. Kawata, T. Goto, Y. Kakefuda, T. Komeda

研究成果: Article査読

16 被引用数 (Scopus)

抄録

The characteristic energy band values such as the Fermi-level position with respect to valence band top for a boron-doped p-type hydrogen-terminated chemical-vapor-deposition (CVD) diamond (0 0 1)2 × 1 surface and for a clean CVD diamond (0 0 1)2 × 1 surface have been determined by a new method with an accuracy of ±0.02 eV. The electron attenuation length for the clean diamond (0 0 1)2 × 1 surface for the electron kinetic energy of C 1s X-ray photoemission peak by Mg Kα excitation is experimentally determined to be 2.1-2.2 nm. These values are compared and discussed with the previously reported experimental and simulation values.

本文言語English
ページ(範囲)860-866
ページ数7
ジャーナルSurface Science
603
6
DOI
出版ステータスPublished - 2009 3月 15

ASJC Scopus subject areas

  • 凝縮系物理学
  • 表面および界面
  • 表面、皮膜および薄膜
  • 材料化学

フィンガープリント

「Characteristic energy band values and electron attenuation length of a chemical-vapor-deposition diamond (0 0 1)2 × 1 surface」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。