TY - JOUR
T1 - Effect of transverse compressive stress on internal reinforced Nb 3Sn superconducting wires and coils
AU - Nishijima, Gen
AU - Watanabe, Kazuo
AU - Araya, Tadahiro
AU - Katagiri, Kazumune
AU - Kasaba, Koichi
AU - Miyoshi, Kazutomi
PY - 2005/10/1
Y1 - 2005/10/1
N2 - Lorentz force is applied to coil windings when the magnet is charged. The coil windings are subjected to huge hoop tensile stress and transverse compressive stress in both the radial and axial directions due to the Lorentz force. The higher the magnetic field and the larger the bore, the larger the Lorentz force applied to the coil windings. Thus, not only the hoop stress, but also transverse compressive stress should be taken into account when designing the magnet. In this paper, we focus on transverse compressive stress, and the influence of this stress on critical current is explored for a standard Nb 3Sn wire and a Cu-NbTi-reinforced Nb3Sn wire. It was confirmed that Cu-NbTi sufficiently reinforced the superconducting wire, not only for tensile stress, but also for transverse compressive stress. The effect of reinforcement arrangement in the cross section was also investigated. In the case that Cu-NbTi reinforcement is arranged at the center of the wire, there was less deterioration in superconducting property than in the case of the reinforcement being arranged in the outer part of the wire.
AB - Lorentz force is applied to coil windings when the magnet is charged. The coil windings are subjected to huge hoop tensile stress and transverse compressive stress in both the radial and axial directions due to the Lorentz force. The higher the magnetic field and the larger the bore, the larger the Lorentz force applied to the coil windings. Thus, not only the hoop stress, but also transverse compressive stress should be taken into account when designing the magnet. In this paper, we focus on transverse compressive stress, and the influence of this stress on critical current is explored for a standard Nb 3Sn wire and a Cu-NbTi-reinforced Nb3Sn wire. It was confirmed that Cu-NbTi sufficiently reinforced the superconducting wire, not only for tensile stress, but also for transverse compressive stress. The effect of reinforcement arrangement in the cross section was also investigated. In the case that Cu-NbTi reinforcement is arranged at the center of the wire, there was less deterioration in superconducting property than in the case of the reinforcement being arranged in the outer part of the wire.
KW - Critical current (C)
KW - Cu-NbTi reinforcement (A)
KW - Lorentz force (C)
KW - NbSn (A)
KW - Transverse compressive stress (C)
UR - http://www.scopus.com/inward/record.url?scp=27744584234&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=27744584234&partnerID=8YFLogxK
U2 - 10.1016/j.cryogenics.2005.08.003
DO - 10.1016/j.cryogenics.2005.08.003
M3 - Article
AN - SCOPUS:27744584234
SN - 0011-2275
VL - 45
SP - 653
EP - 658
JO - Cryogenics
JF - Cryogenics
IS - 10-11
ER -