TY - JOUR
T1 - Precipitation during γ-ε phase transformation in biomedical co-cr-mo alloys fabricated by electron beam melting
AU - Ueki, Kosuke
AU - Kasamatsu, Motoka
AU - Ueda, Kyosuke
AU - Koizumi, Yuichiro
AU - Wei, Daixiu
AU - Chiba, Akihiko
AU - Narushima, Takayuki
N1 - Funding Information:
Funding: This study was financially supported by the Japan Society for the Promotion of Science KAKENHI (grant numbers JP 19K23580, 18H01718, 18H03834 and 17H01329).
Funding Information:
Acknowledgments: This work was partly supported by the “Creation of Life Innovation Materials for Interdisciplinary and International Researcher Development” project. The authors would like to thank K. Kobayashi of Tohoku University for the TEM analyses.
Publisher Copyright:
© 2020 by the authors. Licensee MDPI, Basel, Switzerland.
PY - 2020/1
Y1 - 2020/1
N2 - We studied the precipitates that were induced during γ-ε phase transformation in biomedical Co-28Cr-6Mo (mass%) alloys that were fabricated by electron beam melting with carbon contents of 0.184 and 0.018 mass%. In the high-C as-built alloy, M23X6-type, π-phase (M3T2X-type), and η-phase (M6X-M12X-type) precipitates were observed (M and T: metallic elements, X: C and/or N). σ-phase (Co(Cr,Mo)), π-phase, and Co3Mo2Si-type precipitates were observed in the low-C as-built alloy. This is the first report that shows the presence and chemical composition of this precipitate, as the Co3Mo2Si-type precipitate has not been detected in biomedical Co-Cr-Mo alloys before. After aging in the ε-phase stability region, the high-C and low-C alloys both contained a single ε-phase matrix, and the amount of π-phase precipitates increased. Conversely, the amount of π-phase precipitates in both alloys decreased when a reverse transformation treatment was applied in the γ-phase stability region after aging. In the low-C alloy, the amount of Co3Mo2Si-type precipitates increased after reverse transformation treatment. These results indicate that the dissolution of π-phase precipitates and the formation of Co3Mo2Si-type precipitates during reverse transformation promote the formation of fine γ-phase grains at the precipitate/ε-phase matrix interface, because the formation and dissolution of these precipitates affect the γ-phase stability of the matrix.
AB - We studied the precipitates that were induced during γ-ε phase transformation in biomedical Co-28Cr-6Mo (mass%) alloys that were fabricated by electron beam melting with carbon contents of 0.184 and 0.018 mass%. In the high-C as-built alloy, M23X6-type, π-phase (M3T2X-type), and η-phase (M6X-M12X-type) precipitates were observed (M and T: metallic elements, X: C and/or N). σ-phase (Co(Cr,Mo)), π-phase, and Co3Mo2Si-type precipitates were observed in the low-C as-built alloy. This is the first report that shows the presence and chemical composition of this precipitate, as the Co3Mo2Si-type precipitate has not been detected in biomedical Co-Cr-Mo alloys before. After aging in the ε-phase stability region, the high-C and low-C alloys both contained a single ε-phase matrix, and the amount of π-phase precipitates increased. Conversely, the amount of π-phase precipitates in both alloys decreased when a reverse transformation treatment was applied in the γ-phase stability region after aging. In the low-C alloy, the amount of Co3Mo2Si-type precipitates increased after reverse transformation treatment. These results indicate that the dissolution of π-phase precipitates and the formation of Co3Mo2Si-type precipitates during reverse transformation promote the formation of fine γ-phase grains at the precipitate/ε-phase matrix interface, because the formation and dissolution of these precipitates affect the γ-phase stability of the matrix.
KW - Additive manufacturing
KW - Co-Cr-Mo alloy
KW - Heat treatment
KW - Reverse transformation treatment
UR - http://www.scopus.com/inward/record.url?scp=85077559737&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=85077559737&partnerID=8YFLogxK
U2 - 10.3390/met10010071
DO - 10.3390/met10010071
M3 - Article
AN - SCOPUS:85077559737
SN - 2075-4701
VL - 10
JO - Metals
JF - Metals
IS - 1
M1 - 71
ER -