title = "Production of tantalum fine powder by reduction of tantalum chloride with zinc",
abstract = "Reduction of tantalum chloride (TaCI5) with metallic zinc (Zn) was studied by means of injecting TaCI5 into NaCl-LiCl or LiCl-KCl molten salts together with the carrier gas (Ar) through the injection tube. Experiments were carried out in the temperature range of 673-973K. As the reaction and deposition was limited in the molten salts as a reaction medium, recovery of the product was easier compared with the past study in which gas phase was used as a reaction medium. Tantalum fine powder with primary particle smaller than 1 μm was obtained in any condition. Also the particle was much sintered compared with those from the gas phase reaction.",
author = "Yosuke Hoshino and Osamu Takeda and Masayoshi Hoshi and Yuzura Sato",
year = "2009",
doi = "10.1149/1J159329",
language = "English",
isbn = "9781615676422",
series = "ECS Transactions",
publisher = "Electrochemical Society Inc.",
number = "49",
pages = "247--253",
booktitle = "ECS Transactions - Molten Salts and Ionic Liquids 16 - 214th ECS Meeting",
edition = "49",
note = "Molten Salts and Ionic Liquids 16 - 214th ECS Meeting ; Conference date: 12-10-2008 Through 17-10-2008",
}